| Bulkdichtheid | 10,80 g/cm3 |
|---|---|
| Samendrukkracht | Mpa 100 |
| Buigkracht | 50 MPa |
| elektrische weerstand | 11~13 μΩ.m |
| Kusthardheid | 60 HSD |
| Bulkdichtheid | 10,80 g/cm3 |
|---|---|
| Samendrukkracht | Mpa 100 |
| Buigkracht | 52 Mpa |
| elektrische weerstand | 11~13 μΩ.m |
| Kusthardheid | 60 HSD |
| Bulkdichtheid | 10,85 g/cm3 |
|---|---|
| Samendrukkracht | 115 Mpa |
| Buigkracht | 55 MPa |
| elektrische weerstand | 13~14 μΩ.m |
| Kusthardheid | 70 HSD |
| Bulkdichtheid | 10,80 g/cm3 |
|---|---|
| Samendrukkracht | Mpa 100 |
| Buigkracht | 52 Mpa |
| elektrische weerstand | 11~13 μΩ.m |
| Kusthardheid | 60 HSD |
| Bulkdichtheid | 10,80 g/cm3 |
|---|---|
| Samendrukkracht | Mpa 100 |
| Buigkracht | 52 Mpa |
| elektrische weerstand | 11~13 μΩ.m |
| Kusthardheid | 60 HSD |
| Bulkdichtheid | 10,85 g/cm3 |
|---|---|
| Samendrukkracht | 115 Mpa |
| Buigkracht | 55 MPa |
| elektrische weerstand | 13~14 μΩ.m |
| Kusthardheid | 70 HSD |
| Smeltepunt | 3652°C |
|---|---|
| Zuiverheid | 990,9% |
| Vorm | Poeder |
| Materiaal | Grafiet |
| Hardheid | 75 HS |
| Partikelgrootte | 6 micron |
|---|---|
| Zuiverheid | 99.99% |
| Applicatietemperatuur | tot en met 3000°C |
| Warmtegeleidbaarheid | 125 W/mK |
| Dichtheid | 10,85 g/cm3 |
| Bulkdichtheid | 10,80 g/cm3 |
|---|---|
| Samendrukkracht | Mpa 100 |
| Buigkracht | 50 MPa |
| elektrische weerstand | 11~13 μΩ.m |
| Kusthardheid | 60 HSD |
| Bulkdichtheid | 10,85 g/cm3 |
|---|---|
| Samendrukkracht | 115 Mpa |
| Buigkracht | 55 MPa |
| elektrische weerstand | 13~14 μΩ.m |
| Kusthardheid | 70 HSD |